  • L
    Hi, Look at this thread. Best to read all of the parts about staining, carving, silver wire, and finishing...
  • L
    LRB replied to the thread Spring making.
    In an oven, maybe an hour. In lead 15/20 minutes seem enough because the steel has full contact with the heat. The thickness off the...
  • L
    LRB replied to the thread Spring making.
    Usually only air hardening steels require foil protection or advanced atmosphere protection. Coatings such as ATP-641 are good at...
  • L
    LRB replied to the thread Spring making.
    Not long ago many DIY at home blade makers used toaster ovens for the temper process. It seems they worked reasonably well but there...
  • L
    LRB reacted to FlinterNick's post in the thread Spring making with Like Like.
    Facebook market place
  • L
    LRB replied to the thread Spring making.
    It only works well when done at midnight on a full moon while chanting Bibbidi bobbidi boo over the boiling oil.