• Friends, our 2nd Amendment rights are always under attack and the NRA has been a constant for decades in helping fight that fight.

    We have partnered with the NRA to offer you a discount on membership and Muzzleloading Forum gets a small percentage too of each membership, so you are supporting both the NRA and us.

    Use this link to sign up please; https://membership.nra.org/recruiters/join/XR045103

Dental X-Ray Lead strips.

Muzzleloading Forum

Help Support Muzzleloading Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Joined
Jul 6, 2021
Messages
678
Reaction score
1,025
Location
SC
I was given 11 lbs. of lead strips previous.y attached to dental X ray tabs. Melted it down, fluxed it. An incredible amount of black crumbly dross appeared on the surface. Poured into 1 lb. Ingots, the last two have strange color and 1 cracked in half, large grain appeared. Thinking zinc may have been present in product. Anyone else ever used any of these?
 
Yes, this is what I have been casting all my ball with. My cousin is a dentist, and saves them for me.

I have been using a Lee production pot with the bottom pour.

I do not add flux, just drop the backings right in.

I, too, have encountered the crumbly dross. I just keep it skimmed and keep pouring.

I have not tested hardness for presence of alloys, but it shoots great in my rifles.

I have not poured any ingots, just straight into ball/minie moulds.
 
I used these for many years. Be sure the black paper backing sheet is removed from the lead portion of the x-ray backer.

I also had a cousin who was a dentist, and saved them for me. Recently sold the last 30#.
 
Theoritcal weight of a .495 lead sphere in 184.2gr. My .495 cast ball weighed 183.5 gr (less than 4 thousandths of a percent difference), and showed good weave marks from the patch when I pulled a ball. Plenty soft to shoot, and win my fair share of matches.
 