A long time ago I gave up the idea of using pyrate
because of what I heard. Others were using welders
flint [ferriseum sic]. I had pretty good luck with
them until now when I contacted FireSteel.com and
ordered several 3/16 X 3" sticks. I cut them to
size and insert in a brass block in the jaws of
the dog..Very hot compared to what I had used...I
can get ten flashes in a row and that is only because
I stopped there. These Fire sticks last very long
and I rotate them a quarter turn every few shots..
I am very satisfied and will continue using them.
Very inexpensive AND very available.Contact Ron
Fontaine at FireSteel.com. He has various sizes
and lengths...I hope I didn't break any rules with that address.
Wulf
because of what I heard. Others were using welders
flint [ferriseum sic]. I had pretty good luck with
them until now when I contacted FireSteel.com and
ordered several 3/16 X 3" sticks. I cut them to
size and insert in a brass block in the jaws of
the dog..Very hot compared to what I had used...I
can get ten flashes in a row and that is only because
I stopped there. These Fire sticks last very long
and I rotate them a quarter turn every few shots..
I am very satisfied and will continue using them.
Very inexpensive AND very available.Contact Ron
Fontaine at FireSteel.com. He has various sizes
and lengths...I hope I didn't break any rules with that address.