• Friends, our 2nd Amendment rights are always under attack and the NRA has been a constant for decades in helping fight that fight.

    We have partnered with the NRA to offer you a discount on membership and Muzzleloading Forum gets a small percentage too of each membership, so you are supporting both the NRA and us.

    Use this link to sign up please; https://membership.nra.org/recruiters/join/XR045103

Cherry Stocks: Traditional Long Rifle Finishes

Muzzleloading Forum

Help Support Muzzleloading Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
The first test piece I used was one teaspoon of lye to 15 ounces of water which did color but not as much as I had hoped. I upped the ante by an extra teaspoon to the previous mixture and started getting darker results. The key to getting a deeper red color is to blush the wood with a heat gun like Rich Pierce suggested.
Do you blush it with the heat gun after the lye solution dries?
 
Do you blush it with the heat gun after the lye solution dries?
How I did it. I applied the lye mixture, immediately blushed it with heat, and then neutralized it with vinegar. I've read that some folks let it dry overnight and then blushed it with heat, so I may try that next to see if it will offer any differences.
 
How do you account for the natural darkening of the cherry ? I have some natural Cherry furniture and it definitely ages or “tans “ when exposed to the sun .
Most of the finishes used on rifles are not UV shielding so I suspect if your stock is in the sun it would darken naturally ?
 