Grenadier1758 Cannon MLF Supporter Joined Oct 9, 2004 Messages 11,965 Reaction score 13,135 Location St. Louis, MO Aug 10, 2021 #21 Melt them down with a lot of known pure lead and molded into a ball sized for relatively easy loading.
Melt them down with a lot of known pure lead and molded into a ball sized for relatively easy loading.
tom_in_vt 45 Cal. MLF Supporter Joined Jul 27, 2021 Messages 513 Reaction score 413 Location NEK, VT Aug 13, 2021 #22 I’d go pure lead, a little antimony if you’re having trouble filling the mold out.
Woody Morgan 62 Cal. Joined Jan 19, 2021 Messages 1,677 Reaction score 2,636 Location Very NW Florida Aug 13, 2021 #23 tom_in_vt said: I’d go pure lead, a little antimony if you’re having trouble filling the mold out. Click to expand... A little tin would work much better. wm
tom_in_vt said: I’d go pure lead, a little antimony if you’re having trouble filling the mold out. Click to expand... A little tin would work much better. wm
ord sgt .58 cal MLF Supporter Joined Jan 9, 2008 Messages 1,953 Reaction score 2,225 Location Socialist state of southern New Jersey Aug 13, 2021 #24 If you can make a mark in the lead with your fingernail, the lead is soft enough to cast roundball for rifle or pistol.
If you can make a mark in the lead with your fingernail, the lead is soft enough to cast roundball for rifle or pistol.
nhmoose 58 Cal. MLF Supporter Joined Sep 30, 2010 Messages 5,872 Reaction score 4,309 Location North of Golden Pond, NH, USA Aug 24, 2021 #25 To not make a rule violation I cannot give you a link to help you. rule #28: Do not post links to sites that contain Muzzleloading Forums. Send me a conversation
To not make a rule violation I cannot give you a link to help you. rule #28: Do not post links to sites that contain Muzzleloading Forums. Send me a conversation