• Friends, our 2nd Amendment rights are always under attack and the NRA has been a constant for decades in helping fight that fight.

    We have partnered with the NRA to offer you a discount on membership and Muzzleloading Forum gets a small percentage too of each membership, so you are supporting both the NRA and us.

    Use this link to sign up please; https://membership.nra.org/recruiters/join/XR045103

making tang fit with heat

Muzzleloading Forum

Help Support Muzzleloading Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

ffg

58 Cal.
MLF Supporter
Joined
Oct 27, 2009
Messages
224
Reaction score
162
Location
ARIZONA
Need to make my GPR kit tang 1/8" longer to fit the tang channel. Has anyone ever heated up and peened a tang to make it a tad longer.This is my 3rd GPR with the same over inletted tang channel.
 
1/8 inch sounds like a lot to me.

Are you sure the hooked breech block isn't hanging up on some interference with the wood down in the rear of the barrel channel? It doesn't take much to cause the metal parts to fail to seat where they should be.

My second thought was, "Can you return the stock to the place that sold it to you?"

That much mismatch (assuming the breech block is fully seated where it should be) is intolerable and the company that makes these should make it right.
 
Yes, you can stretch a tang out longer, if you hit it from underneath with a cross-peen hammer, but of course it'll have to be a trifle thinner in spots. If the tang is long, you can give it a strike every half inch or so, at room temperature, and measure carefully how it lengthens. Its easier to do than explain...
 