I've been using a 1:5 ratio castor oil : denatured alcohol mix for treating fiber wads for use with roundballs in my .62 fusil. They work great, and loading is smooth throughout an entire day of shooting without need for any swabbing.
I wanted to try olive oil, but found it's not soluble in DA. I mixed 1:5 olive oil : napthalene, and have some wads out in the sun now to evaporate off the napthalene. If these work as well as the castor oil, olive oil and Coleman Fuel are both cheaper.