hi all, was trying to find Dave Persons post on strengthening thin forearms with pro bed 2000. i have a kibler fowler i want to do this to. does anyone remember what he thinned it with. thanks in advance. mike
This may be what you are looking for.hi all, was trying to find Dave Persons post on strengthening thin forearms with pro bed 2000. i have a kibler fowler i want to do this to. does anyone remember what he thinned it with. thanks in advance. mike
I use nothing but original jb weld. Acraglass is too expensive, dries out before you can fully use it and not as good as jb weld. Had too many problems with it not fully curing.is there any reason that regular epoxy resin could not be used? is acraglas something special??
Self bowyer's use a sealant called "Massie finish". So named because it was popularized by a fellow named Massie.hi frontiers, not looking to bed the barrel , a very thin coat of thinned epoxy is brushed on to soak into to the wood to reinforce it.